ASTM D3826 is a tensile test method, which covers a degradation - end point, or a brittle point) for degradable polyethylene/polypropylene control-insistent pang and sheeting less than 1.0 mm thick.
Before conducting ASTM D3826, it is important to read the - specification. The Standards can be obtained from the appropriate standard authorities.